MedPotWearPatternID,Term,Description,UseIndicated,MoorhouseReference,DataEnteredOn,DataUpdatedBy 1,1,"on edge and top of rim","heated with a lid in position",1,"2006-06-01 00:00:00","dbmanagement" 2,2,"zone around neck","heated with a lid in position",2,"2006-06-01 00:00:00","dbmanagement" 3,3,"on edge and top of rim and zone above shoulder","heated with a lid in position",3,, 4,4,"around edge and underside of rim","suspended in boiling water contained in a cauldron",4,, 5,5,"around top two-thirds of pot but not on top of rim","heated with a lid in position",5,, 6,6,"on underside of base and lower walls","-",6,, 7,7,"on walls from just above shoulder to base","-",7,, 8,8,"around basal angle","-",8,, 9,9,"lower vessel walls but clean just above basal angle","Sat on the rim of another pot or sat within a griddle",9,, 10,10,"underside of base","-",10,, 11,11,"top, edge and underside of rim and on underside of base and lower walls","-",11,, 12,12,"underside of base and on walls up to shoulder","-",12,, 13,13,"Underside of base, entire external surface apart from top of rim","-",13,, 14,14,"Zone around lower walls ending abruptly at basal angle","-",14,, 15,15,"Around lower walls","-",15,, 16,16,"Inside neck","-",16,, 17,17,"Inside base","-",17,, 18,18,"Entire internal surface","Combustion inside pot",18,, 19,19,"Entire internal and external surface apart from top of rim","Combustion inside pot",19,, 20,20,"Inside of base, underside of base and well-defined narrow band just above basal angle","Charcoal used as fuel",20,, 21,21,"Sooting up to shoulder and around rim","Heated in or at the edge of a wood-burning fire",0,, 22,41,"On rim and around edge of rim","External lid",1,, 23,42,"Rim edge and around underside on rim","External lid",2,, 24,43,"Wear around inside of neck","Internal lid",3,, 25,44,"Zone around girth","-",4,, 26,45,"Underside of base","Contact with hard surface",5,, 27,46,"Around basal angle","-",6,, 28,47,"Area of basal angle","Tilting during pouring if below spout or opposite rim",7,, 29,61,"post-firing modification",,,"2008-10-29 00:00:00","medpot" 30,70,"buff-coloured sherds","under-firing",,"2008-11-20 00:00:00","medpot" 31,71,"warping","over-firing",,"2008-11-20 00:00:00","medpot" 32,72,"Dents","forming/pre-firing fault",,"2008-11-20 00:00:00","medpot" 33,73,"cracking","firing fault",,"2008-11-20 00:00:00","medpot" 34,74,"lamination","forming/firing fault",,"2008-11-20 00:00:00","medpot" 35,75,"upper handle attachment coming away from neck","forming fault",,"2008-11-20 00:00:00","medpot" 36,76,"vessel walls too thin","forming fault",,"2008-11-20 00:00:00","medpot" 37,77,"splashes of glaze on coarse ware vessels esp around neck","firing fault",,"2008-12-10 00:00:00","medpot" 38,78,"clay adhesions",,,"2008-12-03 00:00:00","medpot" 39,79,"matt glaze (on fine wares)","glaze prep/firing",,"2008-12-10 00:00:00","medpot" 40,80,"blistered or bubbled glaze","glaze fault",,"2008-12-11 00:00:00","medpot" 41,81,"glaze on breaks","firing fault",,"2008-12-11 00:00:00","medpot" 43,82,"horizontal break lines (along lines of weakness)","forming fault",,"2009-03-25 00:00:00","medpot" 44,83,"columns of surface cracking (laddered tights effect)","?water leaking into kiln",,"2009-03-25 00:00:00","medpot" 45,84,"pebble in clay causing breakage","poor clay preparation",,"2009-03-25 00:00:00","medpot" 46,85,"air in clay","poor clay preparation",,"2009-03-25 00:00:00","medpot" 47,86,"untrimmed finish, e.g holes of holed bowls and bases","poor quality control",,"2009-04-07 00:00:00","medpot" 48,87,"iron or other (non-clay) adhesions","?post-depositional",,"2009-05-05 00:00:00","medpot" 49,88,"accidentally reduced (for fine wares)","firing fault",,"2009-06-11 00:00:00","medpot" 50,89,"burnt","firing or post-firing",,"2009-06-17 00:00:00","medpot" 51,90,"repair pad","forming fault",,"2009-10-29 00:00:00","medpot" 52,91,"glaze creep","glazing fault",,"2009-10-29 00:00:00","medpot"